Kool Mu powder cores are made of a ferrous alloy powder, which has low losses at elevated temperatures. Kool Mu E-cores have a distributed air gap which makes them ideally suited for switching regulator inductors, flyback transformers, and power factor correction (PFC) inductors. The 10,500 gauss saturation level of Kool Mu provides a higher energy storage capability than can be obtained with gapped ferrite E-cores, resulting in smaller core size. Kool Mu E-cores are competitively priced against gapped ferrite E-cores and their distributed air gap eliminates gap loss problems associated with ferrites. Kool Mu E-cores have significantly lower losses and substantially better thermal properties when compared to powdered iron E-cores.

For complete technical information regarding material characteristics, refer to the Powder Cores Design Manual and Catalog.

 

Special Advantages of MAGNETICS® Kool Mu E-cores
  • E-shaped geometry is manufactured exclusively by MAGNETICS
  • the distributed air gap results in a soft inductance versus DC bias curve
  • available in four permeabilities, 26µ, 40µ, 60µ, and 90µ
  • significantly better DC bias characteristics than gapped ferrites
  • higher energy storage capacity than ferrite, allowing the use of a smaller core
  • excellent performance over temperature
  • lower core losses compared to powdered iron
  • Visit the toroidal Kool Mu page for a more in-depth discussion of Kool Mu material advantages.